Quantity: | |
---|---|
Sort | Color | Plating thickness | Temerature | Salt spray test | Remarks |
Zinc | Silver/Blue/ Multicolour/Black | 10-20 | ≤160° | >48hr | Applied to a wild rangeof products,the deeper cilour the better salt spray resistance |
Nickel plating | Silver | 10-30 | ≤200° | >48hr | Applied to a wild range of products |
NI-CO-NI | Silver | 20-30 | ≤200° | >72hr | Salt spray-resistance wet and heat resistance |
Epoxy | Black | 10-30 | ≤120° | >96hr | Well climate and salt spray resistance |
Nickel | Dull silver | 5-30 | ≤200° | >200hr | Applied to various shape and pated deep inner hole |
Aluminium hydronium | Silver white | 10-30 | ≤400° | >200hr | Average coating,exellent adhesion to the magnetic field and no shielded |
Parylene | Clarity | 5-30 | ≤200° | >200hr | Average coating,exellent adhesion to the magnetic field and no shielded |
Sort | Color | Plating thickness | Temerature | Salt spray test | Remarks |
Zinc | Silver/Blue/ Multicolour/Black | 10-20 | ≤160° | >48hr | Applied to a wild rangeof products,the deeper cilour the better salt spray resistance |
Nickel plating | Silver | 10-30 | ≤200° | >48hr | Applied to a wild range of products |
NI-CO-NI | Silver | 20-30 | ≤200° | >72hr | Salt spray-resistance wet and heat resistance |
Epoxy | Black | 10-30 | ≤120° | >96hr | Well climate and salt spray resistance |
Nickel | Dull silver | 5-30 | ≤200° | >200hr | Applied to various shape and pated deep inner hole |
Aluminium hydronium | Silver white | 10-30 | ≤400° | >200hr | Average coating,exellent adhesion to the magnetic field and no shielded |
Parylene | Clarity | 5-30 | ≤200° | >200hr | Average coating,exellent adhesion to the magnetic field and no shielded |