Quantity: | |
---|---|
High Quality 3*1 SmCo magnet
Material | 35% Sm, 60% Co and 5% Fe & Cu | |
Working | Grade | Max. Operating Temperature |
| XG16-XG22 | 250°C (482°F) |
| XG16H-XG22H | 250°C (482°F) |
| XGS24-XG32 | 350°C (662°F) |
| XGS24M-XG32M | 350°C (662°F) |
| XGS24H-XG32H | 350°C (662°F) |
Shape | Disc, Cylinder, Block, Ring, Countersunk, Segment shapes and more. Customized shapes for SmCo Magnets are available. | |
Size | 1.Block / Bar Length x Width x Thickness 2.Disc / Cylinder Diameter x Thickness 3.Ring Outer Diameter x Inner Diameter x Thickness 4. According to the design | |
Directions of | 1.Oriented through thickness 2.Axially oriented 3.Axially oriented in segments 4.Oriented laterally multipole on one face 5.Multipole oriented in segments on outside diameter 6.Multipole oriented in segments on one face 7.Radially oriented ; Or-rented through diameter Multipole oriented in segments on inside diameter | |
Application | SmCo Magnets All sorts of SmCo are used in the electronic magnetron, magnetic transmission, magnetic treatment etc. |
High Quality 3*1 SmCo magnet
Material | 35% Sm, 60% Co and 5% Fe & Cu | |
Working | Grade | Max. Operating Temperature |
| XG16-XG22 | 250°C (482°F) |
| XG16H-XG22H | 250°C (482°F) |
| XGS24-XG32 | 350°C (662°F) |
| XGS24M-XG32M | 350°C (662°F) |
| XGS24H-XG32H | 350°C (662°F) |
Shape | Disc, Cylinder, Block, Ring, Countersunk, Segment shapes and more. Customized shapes for SmCo Magnets are available. | |
Size | 1.Block / Bar Length x Width x Thickness 2.Disc / Cylinder Diameter x Thickness 3.Ring Outer Diameter x Inner Diameter x Thickness 4. According to the design | |
Directions of | 1.Oriented through thickness 2.Axially oriented 3.Axially oriented in segments 4.Oriented laterally multipole on one face 5.Multipole oriented in segments on outside diameter 6.Multipole oriented in segments on one face 7.Radially oriented ; Or-rented through diameter Multipole oriented in segments on inside diameter | |
Application | SmCo Magnets All sorts of SmCo are used in the electronic magnetron, magnetic transmission, magnetic treatment etc. |
Curie Temp. | Tc | °C | 800-850 | Coeff. Of thermal expansion | C // | 1/°C | ~8×10-5 |
Density | D | g/cm3 | 8.3-8.5 | C⊥ | 1/°C | ~11×10-5 | |
Recoil permeability | rec | 1.00-1.05 | Regidity Strength | N/m2 | ~1.5×108 | ||
Max.working Temp. | Tmax | °C | 350 | Compress Strength | N/m2 | ~8×108 | |
Electrical Resistivity | ΩCm | ~8.6×10-5 | Tensile Strength | N/m2 | ~3.5×107 | ||
Vickers Hardness | Hv | 500-600 | Young’s modulus | N/m2 | ~1.2×1011 | ||
Thermal Conduct Rate | W/mK | ~12 | Magnetization field Ha | kA/m | ≥1600 |
Welcome to contact us ,we are 24 hours on line:
Trade Manager:chinasupergroup
Cell phone:86+13855156049 86+18009691660
Skype:rainbow0051
Curie Temp. | Tc | °C | 800-850 | Coeff. Of thermal expansion | C // | 1/°C | ~8×10-5 |
Density | D | g/cm3 | 8.3-8.5 | C⊥ | 1/°C | ~11×10-5 | |
Recoil permeability | rec | 1.00-1.05 | Regidity Strength | N/m2 | ~1.5×108 | ||
Max.working Temp. | Tmax | °C | 350 | Compress Strength | N/m2 | ~8×108 | |
Electrical Resistivity | ΩCm | ~8.6×10-5 | Tensile Strength | N/m2 | ~3.5×107 | ||
Vickers Hardness | Hv | 500-600 | Young’s modulus | N/m2 | ~1.2×1011 | ||
Thermal Conduct Rate | W/mK | ~12 | Magnetization field Ha | kA/m | ≥1600 |